Tuesday, October 26, 2010

Making Tetrax in GBP, Pondicherry 2010













Well, clay n cracks are synonyms in my case, I guess.





A lot of artists do, and I have also exaggerated cracks out of aesthetic choice.







Though in this piece any deformation in the shape is not acceptable.





It bisque-fired successfully.




There were a few surface cracks.


We decided to barely move the piece and glaze it on the kiln bed.


I had prepared a pattern which I sketched and glazed it.


No comments:

Post a Comment